Per the study “Mechanical properties of modern restorative ‘bioactive’ dental materials” (Scientific Reports):
Flexural strength: median 120.40 MPa — the highest among bioactive materials tested.
Modulus of elasticity: 7.27 ± 0.78 GPa
Diametral tensile strength: 47.08 MPa
Vickers hardness (baseline): approximately 47.0–48.8 HV